METHOD FOR PRODUCING GLASS FIBER-REINFORCED RECYCLED POLYPHENYLENE SULFIDE RESIN COMPOSITION, AND MOLDED ARTICLE OBTAINED BY MOLDING GLASS FIBER-REINFORCED RECYCLED POLYPHENYLENE SULFIDE RESIN COMPOSITION
Fuente:
WIPO "circular economy"
A method of producing a glass fiber-reinforced recycled PPS resin composition, including: crushing a molded product containing a polyphenylene sulfide resin and glass fibers to obtain a crushed molded product (A), and mixing the crushed molded product (A) and a PPS resin composition (B) containing 40 to 90 wt% of the PPS resin having a weight average molecular weight of 20,000 to 60,000 and 10 to 60 wt% of glass fibers. The present invention provides a glass fiber-reinforced recycled PPS resin composition which suppresses breakage of glass fibers at the time of recycling the glass fiber-reinforced PPS resin composition, and has excellent mechanical properties.
Al elegir "Aceptar todas las cookies", acepta el uso de cookies para ayudarnos a brindarle una mejor experiencia de usuario y analizar el uso del sitio web. Al hacer clic en "Ajuste sus preferencias" puede elegir qué cookies permitir. Solo las cookies esenciales son necesarias para el correcto funcionamiento de nuestro sitio web y no pueden ser rechazadas
Configuración de cookies
Nuestro sitio web almacena cuatro tipos de cookies. En cualquier momento puede elegir qué cookies acepta y cuáles rechaza. Puede obtener más información sobre qué son las cookies y qué tipos de cookies almacenamos en nuestra Política de cookies.
Son necesarios por razones técnicas. Sin ellos, es posible que este sitio web no funcione correctamente.
Son necesarios para una funcionalidad específica en el sitio web. Sin ellos, algunas funciones pueden estar deshabilitadas.
Nos permite analizar el uso del sitio web y mejorar la experiencia del visitante
Permítanos personalizar su experiencia y enviarle contenido y ofertas relevantes, en este sitio web y en otros sitios web